Troubleshooting of Circulation Line Blockage for Two-component (2K) Varnish

  • LI Shu-zhen[1];HUA Yun[2]
Author information +
History +

Abstract

The common type of paint transmission system of two-component varnish is introduced.The cause analysis and verification process of blockage for 2K varnish are described.The measures and suggestions to prevent recurrence are found out.

Key words

two-component(2K)varnish;2K semi-gloss varnish;precipitation/blockage