Study on Problem Analysis and Solution During Import Processfor Bright Yellow Color

ZHANG Jin-xing[1];ZHAN Meng[2]

Modern Paint & Finishing ›› 2021, Vol. 24 ›› Issue (9) : 49-52.

PDF(3397 KB)
PDF(3397 KB)
Modern Paint & Finishing ›› 2021, Vol. 24 ›› Issue (9) : 49-52.

Study on Problem Analysis and Solution During Import Processfor Bright Yellow Color

  • ZHANG Jin-xing[1];ZHAN Meng[2]
Author information +
History +

Abstract

The bright yellow color has some properties such as high saturation,high pigmentbinder ratio andpoor hiding power,so three typical problems are found during the import process.For instant,the metamericphenomenon is obvious between D65/10 light source and A/10 light source.Meanwhile the recoating film hasthe risk of peeling off caused by low adhesive force,and it is difficult to balance thin paint and sagging due topoor application property.For these three problems,the causes were analyzed and targeted measures wereproposed.Finally,the above-mentioned typical problems were eliminated through the implementation ofcomprehensive strategies including adjusting paint materials and optimizing construction parameters,and thequality returned stability simultaneously.

Key words

bright yellow color;metameric phenomenon;recoating adhesive force;wettability,applicationproperty of interior spraying

Cite this article

Download Citations
ZHANG Jin-xing[1];ZHAN Meng[2]. Study on Problem Analysis and Solution During Import Processfor Bright Yellow Color[J]. Modern Paint & Finishing. 2021, 24(9): 49-52
PDF(3397 KB)

Accesses

Citation

Detail

Sections
Recommended

/