水性阻尼胶脱落问题的解决

陈忠德[1];曹玲玲[1]

现代涂料与涂装 ›› 2022, Vol. 25 ›› Issue (10) : 48-50.

PDF(1737 KB)
PDF(1737 KB)
现代涂料与涂装 ›› 2022, Vol. 25 ›› Issue (10) : 48-50.

水性阻尼胶脱落问题的解决

  • 陈忠德[1];曹玲玲[1]
作者信息 +

Solution of Shedding Problem of Liquid Applied Sound Deadener

  • CHEN Zhong-de[1];CAO Ling-ling[1]
Author information +
文章历史 +

摘要

针对一起因汽车车内水性阻尼胶(LASD)压线时间久导致材料局部脱落问题的应用案例,对原材料配方、现场施工工艺进行了分析与验证,通过延长材料表干时间、降低发泡剂含量、降低局部烘烤温度及降低膜厚等方法解决了该问题。

Abstract

Aiming at an application case of partial shedding of materials caused by a long pressing time of LASD in automobile,the formulation of raw materials and the construction technology on site were analyzed and verified,and the problems were solved by prolonging the surface drying time of materials,reduce foaming agent content reducing the local baking temperature and reducing the film thickness.

关键词

水性阻尼胶;局部脱落;问题解决

Key words

liquid applied sound deadener;partial loss;problem solving

引用本文

导出引用
陈忠德[1];曹玲玲[1]. 水性阻尼胶脱落问题的解决[J]. 现代涂料与涂装. 2022, 25(10): 48-50
CHEN Zhong-de[1];CAO Ling-ling[1]. Solution of Shedding Problem of Liquid Applied Sound Deadener[J]. Modern Paint & Finishing. 2022, 25(10): 48-50
中图分类号: TQ639   

PDF(1737 KB)

Accesses

Citation

Detail

段落导航
相关文章

/