结合车身电泳底漆膜厚不足问题,分析了该问题的原因,并针对各种原因制定了相应的对策.

Abstract

Combined with the problem of the vehicle body with insufficient film thickness of cathodic electro-deposition(CED)coating,the reasons for the problem were analyzed,and corresponding countermeasures were formulated for various reasons.

关键词

电泳涂装;锆化;泳透力

Key words

electro-deposition;zirconium pretreatment technology;throwing power

引用本文

导出引用
吴为[1];刘海军[1];骆宗伟[1]. 切换TecTalis前处理后电泳底漆膜厚不足问题分析[J]. 现代涂料与涂装. 2022, 25(9): 32-34
WU Wei[1];LIU Hai-jun[1];LUO Zong-wei[1]. Analysis on Vehicle Body with Insufficient Film Thickness of Cathodic Electro-deposition Coating after Switching TecTalis Pretreatment[J]. Modern Paint & Finishing. 2022, 25(9): 32-34
中图分类号: TQ639   

PDF(1953 KB)

Accesses

Citation

Detail

段落导航
相关文章

/