Aiming at the poor drying of electrophoretic film in drying room,the problem was completely solved by management and control the electrophoretic process holes to the chassis frame and transforming the electrophoretic drying room,such as installing air outlet nozzle to adjust the air outlet direction at the bottom,adding floor thermal insulation layer and blocking some air outlets.
SUN Ying[1];DENG Yuan-yuan[1];CAO Zu-jun[1];LUO Lei[1];LIU Wei-bin[1].
Analysis of the Causes and Improvement of PoorDrying of the Electrophoretic Film[J]. Modern Paint & Finishing. 2023, 26(1): 37-39