摘要

在湿式喷漆工艺中,不同类型的过喷清漆经循环水捕捉后返回文丘里过程中,已脱黏的漆渣会在文丘里内产生不同程度的堆积、堵塞问题。本文通过对油漆絮凝剂的位置优化、调节,解决了现场文丘里积渣问题。

Abstract

In the wet spraying process,different types of oversprayed varnish are captured by circulating water and returned to the Venturi process.The debonded paint slag will produce different degrees of accumulation and blockage in the Venturi.By optimizing and adjusting the position of paint flocculant,the problem of venturi slag accumulation on site is solved.

关键词

湿式喷漆;文丘里;油漆絮凝剂

Key words

wet spraying;Venturi;paint flocculant

引用本文

导出引用
王博龙[1];石强[1];胡治文[1];徐德庆[1]. 浅谈湿式喷漆工艺中过喷漆脱黏后文丘里积渣的问题解决[J]. 现代涂料与涂装. 2024, 27(4): 56-58
WANG Bo-long[1];SHI Qiang[1];HU Zhi-wen[1];XU De-qing[1]. Discussion on the Solution to the Problem of Venturi Slag Accumulation after Over-Painting Debonding in Wet Spray Painting Process[J]. Modern Paint & Finishing. 2024, 27(4): 56-58
中图分类号: TQ639   

PDF(1860 KB)

Accesses

Citation

Detail

段落导航
相关文章

/